How to dilute POLYOX WSR-301 PEG 90М to 3% liquid
Diluting POLYOX WSR-301 (Polyethylene Glycol) to a 3% liquid solution involves accurately measuring the amount of the polymer and the solvent (usually water) to achieve the desired concentration. Here's a general procedure to create a 3% solution:
Materials needed:
- POLYOX WSR-301 PEG 90M
- Distilled water (or appropriate solvent)
Steps:
1. **Calculate the amount needed:** The concentration of the final solution is 3%. If you want to prepare a specific quantity (let's say 100 grams), you'll need to calculate the amount of POLYOX WSR-301 and water required.
2. **Determine the amount of POLYOX WSR-301:** For a 3% solution of a total volume of 100 grams, you'd need 3 grams of POLYOX WSR-301 (3% of 100 grams).
3. **Measure the water:** Subtract the weight of POLYOX WSR-301 (3 grams) from the total weight (100 grams), which leaves you with 97 grams of water needed (100 grams total - 3 grams of the polymer).
4. **Weigh the POLYOX WSR-301:** Using a precise scale, measure out 3 grams of POLYOX WSR-301.
5. **Mix with water:** Add the 3 grams of POLYOX WSR-301 to 97 grams of distilled water in a suitable container. Stir thoroughly until the polymer dissolves completely. Make sure the mixing is uniform to achieve a homogeneous solution.
6. **Test the solution:** After mixing, allow the solution to rest and ensure it remains homogeneous. If needed, you can adjust the quantities accordingly for larger or smaller volumes.
Note: Always ensure the equipment used is clean and dry to prevent contamination and accurately measure the amounts to maintain the desired concentration.
Also, keep in mind that this procedure is a general guideline. Always refer to the specific instructions provided by the manufacturer for precise measurements and mixing instructions. Safety data sheets (SDS) and product information may provide further details on handling, dilution, and safety precautions for POLYOX WSR-301.